Hello everyone. I would like some guidance on my experimental setup for my Final year project. I am required to make an experimental setup for my WLAM. I need help on the some equipment's that needs to be bought such as XZ axis moving stage/platform required to conduct layering experiment. I have referred many journals but mostly uses 6- axis robotic arm for movement. The project is under tight budget. For the time being, I have the coolant, wire feeder, Laser welding head, laser power system, and laser controller. Below are some other requirements for the project. Please from your experiences please give me some suggestions on how to pursue this. Max power rated for laser welding head 2kW

For the laser head, we may fixed it vertically but may include a manual/motor adjustable Z-axis movement. We are required to find working distance from laser head to focal point (References to Collimation and Focal lens). We will place the Wire feeder accordingly at appropriate angle 30/40/45 degs.

For wire feeder, Need to consider type of wire feeder, diameter, feeding rate. Our max input for welding head is 2000W. Required shielding gas with controlled flow rate. 99% Argon gas.

Cooling Equipment setup Optical Fibre laser bending radius ( If not mistaken, 100mm)- may need to know how and where to bend

Laser settings ( Laser power, type of laser: Pulse/continuous)There were calculation from journal for wire feed rate and some others from journals for consideration

For main structure, We can use the aluminium column seen last time to build in box shape connected with brackets.

Lastly, we must integrate shielding gas, Wire feeder, Laser power (On/OFF), Water Coolant with PLC or some form of controller to initiate these in sequences
 

Attachments

  • Screenshot 2024-12-08 121638.jpg
    Screenshot 2024-12-08 121638.jpg
    144.8 KB · Views: 0
  • WhatsApp Image 2024-12-08 at 12.13.15_c8907cc2.jpg
    WhatsApp Image 2024-12-08 at 12.13.15_c8907cc2.jpg
    122 KB · Views: 0
  • 1123.jpg
    1123.jpg
    130.3 KB · Views: 0
  • 112.jpg
    112.jpg
    163.9 KB · Views: 0
Replies continue below

Recommended for you

I think a simple linear stage to start with - you have a great number of variables already and reducing the degrees of freedom would allow getting to the process variables faster. If the target is moved then nothing else has to - the gas shield, no worries about bending the fiber, the working distance remains constant. All one needs to do then is to vary the speed of the wire feed and the speed of the target and build essentially a welded rod. Which, at first, seems not remarkable. When you understand how all the other variables affect the process, then it's 2D and 3D time.

Here's a torch version with little 3D required:

When you can reliably make a 1D rod then you are off to making more interesting things.

It would also make enclosing the welder much simpler. Unless you are 80 or 90 years old, losing vision to an experiment is a thing to avoid.
 
Thanks for the advice. I will take it under consideration. I believe that linear stage is much easier for time being. Just having a difficulty finding motorised linear bracket online with my current budget. Will be looking out for it
 