wing skin materials

Status
Not open for further replies.

conscin

Aerospace
Joined
Jan 24, 2011
Messages
3
Location
BR
Considering that Al 7475-T7351 plates have good fatigue and crack growth strength and higher fracture toughness than 2024-T351 and others 7XXX alloys, somebody knows why the majors aircraft makers does not use Al 7475-T7351??
Thanks


 
Without doing any research, my off the cuff guess would be cost.
 
despite what is said of 7475 (high quality, premium selection) i don't think it's fatigue properties are as good as 2024. fracture toughness is a secondary importance on the wingskin, compared to crack growth, and i think it's here that 2xxx beats out 7xxx.

2xxx is my preferred choice for lower wing skins, 7xxx for stringers and spars and upper skins.
 
Please don't double post, or if you do put a link to the original thread and ask folks to post over there.

thread330-299505

Posting guidelines faq731-376 (probably not aimed specifically at you)
What is Engineering anyway: faq1088-1484
 