davidd31415
Electrical
I am investigating what would cause the performance of PTC heaters to degrade.
The heating elements are a PTC carbon paste. After being powered at 14V for anywhere from 200 - 3000 hrs at various temperatures the current draw of the heaters drop from 2A to 1A. The resistance of the heaters increases as well but I do not have data for this.
What might cause a resistor to increase in resistance?
I am beginning to experiment with the heaters but if anyone has insight into what might cause the heater resistance/performance to change, I would appreciate hearing it.
The heating elements are a PTC carbon paste. After being powered at 14V for anywhere from 200 - 3000 hrs at various temperatures the current draw of the heaters drop from 2A to 1A. The resistance of the heaters increases as well but I do not have data for this.
What might cause a resistor to increase in resistance?
I am beginning to experiment with the heaters but if anyone has insight into what might cause the heater resistance/performance to change, I would appreciate hearing it.