Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Why should Bolt holes straddle centrelines of Vessels

Status
Not open for further replies.

Balukv

Petroleum
Feb 1, 2002
3
Why should Bolt holes of flanges straddle centrelines of pressure vessels ? I have noticed them in many standards and fabrication rules.

Another question is on why Anchor Bolts of Skirts/Pressure vessels straddle centrelines.

A reasoning I got was that straddled holes provided more space for bolt removal than when the bolt-holes were in-line with the centrelines. Are there any solid reasons for straddling ?
 
Replies continue below

Recommended for you

I have always been told that, the bolts holes are positioned off centre, so that if a small leak occurs it will not drip on a bolt!
If a bolt is at the bottom of the flange it will experience accelerated corrosion, failure and lead to a major leak.
 
Biggy's answer sounds reasonable but I'm guessing it also has to do with standard convention. If you know the flange you're hooking up to is always going to be two holed then you'll always know how your fitting will be orientated. May not always be necessary, but its a good practice to follow.
 
I agree with HUSH. This is a convention that we all are familiar with. The contractor fabricating adjoining piping can be sure, (unless told otherwise)that his mating flanges must follow that convention in order for the piping to be installed in the right direction. Similarly, the contractor installing holding-down bolts will be familiar with the convention and will install accordingly.

In both cases, straddling the centreline can be more accurately varified because a square can be aligned with the two bolt holes or bolts so that the opposite leg is aligned with the vessel or foundation axis.