Why SA 240 Gr 316L is not listed in Table UHA-44

Status
Not open for further replies.

brkmech1234

Mechanical
Oct 18, 2011
67
I wonder why SA 240 Gr 316L(UNS S31603) is listed in Table UHA-44 of ASME VIII Division 1. Anybody can help in this regard.
 
Replies continue below

Recommended for you

Because it is low carbon and is less susceptible to strain induced carbide precipitation.
 
Thank you for reply. Can you please show me the code reference showing this exemption
 
There is none. The code does not provide reasons for not listing material. The code only provides rules for use of listed material and restrictions on use, if applicable.
 