Because when you gaze at an attractive woman, look deeply into her beautiful eyes, try to say something inteligent and watch her smile........ your heart is not getting cold.

Gimmie a star......

 
My SWAG -- Scientific Wild-A$$ed Guess -- is that in the early days of pipelining, the root was run fairly 'cold' and fast. This closes up the open gap in the root. Then comes a hotter, slower pass to tie everything a little better: the Hot Pass.

If you watch any root when the 2nd [hot] pass is being welded, it does indeed get very hot, and portions of the root may remelt.
 
The hot pass is intended to remelt the root to a certain degree, and thus eliminating any "wagon wheel tracks" that may be present in the root pass.
 