msharief

Civil/Environmental
Apr 18, 2001
14
Why do we get bad results for aggregates abrasion
inspite of good condition of LA abrasion machine
and good calibaration record???.Please give ur
suggestions. Mohammed A Sharief
 
Replies continue below

Recommended for you

msharief...the results, assuming all is well with the equipment as you have stated, are a function of the material properties, most notably the "hardness" of the aggregate.

Are your results excessive as compared to results by another laboratory? Are they excessive compared to results of an aggregate producer?

Please explain what you mean by "bad results".
 
by bad results do you mean inconsistent, random, low or what? in comparison with those from aggregate suppliers or other labs?
 
Thanx Ron and Slow
Low when compared to other labs and 3% variation Mohammed A Sharief
 