Jun 14, 2005 #1 edison123 Electrical Joined Oct 23, 2002 Messages 4,517 Location IN Our customer wants to change tin based white metal to lead based white metal for his 100 MW Hydro generator bearings. What will be the repercussions ? Where can I find info on these bearing metal compositions ? Thx in advance.
Our customer wants to change tin based white metal to lead based white metal for his 100 MW Hydro generator bearings. What will be the repercussions ? Where can I find info on these bearing metal compositions ? Thx in advance.
Jun 14, 2005 1 #2 Carburize Materials Joined Sep 23, 2002 Messages 702 Location US ASTM B23 gives details. The lead based Babbitt Metals have lower strength than the tin base so the load carrying capacity is reduced. Upvote 0 Downvote
ASTM B23 gives details. The lead based Babbitt Metals have lower strength than the tin base so the load carrying capacity is reduced.
Jun 14, 2005 Thread starter #3 edison123 Electrical Joined Oct 23, 2002 Messages 4,517 Location IN Thx carburize. I downloaded the std b23 (though $28 for 3 pages seems a bit stiff). It was quite informative. Upvote 0 Downvote
Thx carburize. I downloaded the std b23 (though $28 for 3 pages seems a bit stiff). It was quite informative.