Ferid999

Student
Dec 7, 2023
7
Hi to all engineers
I do masterbatch good quality and good pigments but i face problem in white masterbatch to sell because tio2 cost us so any solution to reduce and replace tio2 in whute masterbatch to get some result and good price to clients
 
Replies continue below

Recommended for you

Have you tried substituting an opacifier for some of the TiO2?

Good Luck,
Latexman

 
Hi
Not yet sir can you suggest wich one is good ? but the important is it must show that its contains 70tio2 in white masterbatch .
 
Try Arkema's Celocor in the lab and see if it reduces cost and keeps performance.

Let us know how it works out.

Good Luck,
Latexman

 
Mr latexman
Wich one is good for whiteness i found a lot of priducts .
Kindly suggest me wich good for Whitness and wich good for black and also colors
I appreciate your help .
 
I am a generalist in this area. Please contact sales/marketing of the companies offering these products and enquire. They should give you input from their specialists.

Good Luck,
Latexman

 