Oct 11, 2005 #1 ALEXANDRAHARPER Structural Joined Sep 13, 2005 Messages 15 Location MX I AM LOOKING FOR INDICATED VALVE MATERIAL FOR STEAM USE IN A GATE VALVE. PLEASE HELP ME AS SOON AS POSSIBLE.
I AM LOOKING FOR INDICATED VALVE MATERIAL FOR STEAM USE IN A GATE VALVE. PLEASE HELP ME AS SOON AS POSSIBLE.
Oct 11, 2005 1 #2 cliff6361 Materials Joined May 5, 2005 Messages 27 Location US Several materials will work in steam. Much depends upon what the actual conditions are. The best choice for general saturated steam is carbon steel, both cast or forged. Upvote 0 Downvote
Several materials will work in steam. Much depends upon what the actual conditions are. The best choice for general saturated steam is carbon steel, both cast or forged.
Oct 11, 2005 #3 SJones Petroleum Joined Apr 22, 2001 Messages 3,945 Location GB Have a look at ASTM F1565 and see if that provides any help. Steve Jones Materials & Corrosion Engineer http://www.pdo.co.om/pdo/ Upvote 0 Downvote
Have a look at ASTM F1565 and see if that provides any help. Steve Jones Materials & Corrosion Engineer http://www.pdo.co.om/pdo/