I AM LOOKING FOR INDICATED VALVE MATERIAL FOR STEAM USE IN A GATE VALVE. PLEASE HELP ME AS SOON AS POSSIBLE.

 
Several materials will work in steam. Much depends upon what the actual conditions are. The best choice for general saturated steam is carbon steel, both cast or forged.
 