Among thin plastics, sheets and films, that are highly transparent to visible light, which are also best at reflecting or absorbing IR heat?

Are there any spray coatings to enhance a clear plastic surface reflecting even more IR without significantly degrading transparency to visible light?

Thank you for any comments.

 
Replies continue below

Recommended for you

The infrared absorption spectrum of every polymer is available in books and online databases. Search for "FTIR polymer spectrum". Every chemical bond absorbs a specific frequency so you can't have an organic polymer that absorbs no IR. The polymers with least types of bond have big windows where they absorb no IR over that frequency range. E.g. polyethylene and polypropylene.

Coatings can help. For example tin oxide is coated onto the glass in your oven to reflect the heat back in. Search for IR reflective coatings.

Chris DeArmitt PhD FRSC
President