I am dealing with hot forged bar, about 6" OD.
It happens to be 15-5PH, but this should apply to any age hardened alloy.
Which position/orientation will have the lowest impact toughness?
I can think of nine different combination to take impact bars, but I only want to take two.
Which will give me worst case?
Opinions are welcomed, if you have a good reason.
= = = = = = = = = = = = = = = = = = = =