I need to find out some information on heat treating densamet (largely tungsten alloy) but cannot find any information from anywhere, so any information would be good!
Thank you,
cpp01
 
Replies continue below

Recommended for you

cpp01;
I located a web site that lists various grades of Densamet alloys;


If this alloy is what I think it is, it is probably similar to Densalloy. We have used Densalloy for balance weights in low pressure steam turbines. The Densalloy is a sintered tungsten product using either iron-copper or iron-nickel as binders. The increased density of the alloy makes for great balance weight consolidation. However, the Densalloy will corrode in elevated steam temperature service (>700 deg F).

I don't believe this alloy is heat treatable after it is sintered. Someone else may have additional information.
 