Enginerdad

Structural
May 18, 2012
66
I understand deformed WWR is more expensive than smooth, but smooth WWR has a pretty short development length to begin with, so when is the proper to specify deformed?
 
Replies continue below

Recommended for you

Smooth WWR development is from the anchorage at wire intersections only. Deformed WWR development is from both the wire intersection anchorage and the deformations. One reason to use deformed WWR is when the WWR is used in structural concrete as a direct replacement for traditional (deformed) rebar.