I am designing an infill for a section of collapsed brick footing on an old house, and underpinning where it collapsed. (It collapsed due to squatters digging the wall to make more room to live.) I'm not worried about load capacity because the wall carries basically no load.
When can brick infill be considered self-supporting? Meaning how long until the mortar is cured enough to hold itself up if there's no support below it? The hole is only 2' wide, so I'm replacing 3 bricks max width. The underpin width is only 6' wide max, and I'm trying to have the process be as quick as possible for the contractor.
Pic attached.
When can brick infill be considered self-supporting? Meaning how long until the mortar is cured enough to hold itself up if there's no support below it? The hole is only 2' wide, so I'm replacing 3 bricks max width. The underpin width is only 6' wide max, and I'm trying to have the process be as quick as possible for the contractor.