I have a carburised and ground 12L14 shaft with 730+/-50 HV Eht approx. 0.15, mating with a needle bearing. after the test cycle (rotation at 2600 rpm and 1.2mm axial reciprocating at 10cycle/rpm along the 8mm guiding span), there is a worn out marking on the shaft that is of yellowish colour, or to be more exact, looks like bronze colour. What's the explanation to this phenomenon?