what's the difference in ASTM A388 vs ASTM A578 ultrasonic testing ?

Status
Not open for further replies.

hsemus

Petroleum
Joined
Apr 26, 2012
Messages
42
Location
GB
Apart from the accepting criteria, is there any other change in the test procedure.
 
A388 is for forgings, A578 for plain and clad plate
 