There was an exotic car made in the '70's that used a bare stainless steel as the body panels. It was called a Bricklin, and was only made for a few years. Does anyone know what type of stainless was used to skin it with?
 
Replies continue below

Recommended for you

I guess it was the DeLorean that was stainless. Oh well, what was the DeLorean body made of?
 
Yep, it was the DeLorean (haven't you seen Back to the Future?[wink]), and I think the skin was made from brushed 304 or 304L stainless.
 