Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

What type of Nylon? 1

Status
Not open for further replies.

Toxotoxo

Industrial
Mar 13, 2012
6
Does anyone know what type of nylon and rubber is used in this product . It states it is heat resistant to 240˚C/480˚F. Also what is the manufacturing process called in which a plastic is coated in rubber?
 
Replies continue below

Recommended for you

They are typically nylon 6.6. It is the highest melting point of any reasonably affordable nylon with a melting point of 256 deg C. It is also available in food contact and medical grades.

Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
The process you asked about is called over-molding.

It is better to have enough ideas for some of them to be wrong, than to be always right by having no ideas at all.
 
OK

Thanks to ON, I just saw the second part of the question.

The rubber is typically polyurethane and the nylon having the higher melting point is moulded over the PU so it has enough heat to fuse to it.

Regards
Pat