What properties does EN24T have?
 
Hi ChuckNorris

Well EN24 is given as a BS970 817M40 equivalent although I not sure what the T stands for.
If you follow this link and scroll down you will find the yield and tensile stress for the equvialent 817M40 material if that helps.


Regards

desertfox
 
hi again

The T might be for specifying the tensile strength range of the material.

regards

desertfox
 
EN24T: 1 1/2% Nickel Chrome Molybdenum steel
Heat treated to the 'T' range = 55/65 tons/sq in.
 
EN24T / 817M40T is equivalent to AISI 4340 if that helps.
T is, as geoffthehammer said, heat treated to a specific range, in metric 850 to 1000MPa.
 