I am looking for metal which will have a very strong attraction to an electromagnet, and I need a metal that would not grow rust.
The metal needs to be unmagnetized after the electromagnet stop working.
 

TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529


Of course I can. I can do anything. I can do absolutely anything. I'm an expert!
There is a homework forum hosted by engineering.com:
 
No rusting means that either the alloy contains Cr (12% at least) or you plate it with either Cr or Ni.
High attraction means that it has high permeability and saturation values.
And you want a low coercivity.

You might start with a well annealed piece of 409 stainless, and compare other materials to that.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Unless coatings not allowed, rust can be divorced from the material equation.

TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529


Of course I can. I can do anything. I can do absolutely anything. I'm an expert!
There is a homework forum hosted by engineering.com:
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top