tc7
Mechanical
- Mar 17, 2003
- 387
This is a general question pertaining to vibration or sub-harmonic systems for distortion control for welds or machining of MILD steels of the ASTM A36 variety:
One feature that a vendor mentions in regard to their vibration or sub-harmonic system is for "distortion control". They seem to distinguish "distortion control" from stress relief. This may be an important distinction when it comes to weld procedures (ASME or AWS). If viewed as a method to control distortion then perhaps it would not need to be addressed as an essential variable whereas a method of post weld stress relief would most certainly have to be.
But my first question is - what is distortion control? is it a means to prevent stress in weldments thereby precluding the need for PWHT?
Secondly, if a qualified weld procedure on A36 mild steel called for no PWHT and a vibrational stress relief was applied anyway, does this violate the WPS?
Thankyou.
One feature that a vendor mentions in regard to their vibration or sub-harmonic system is for "distortion control". They seem to distinguish "distortion control" from stress relief. This may be an important distinction when it comes to weld procedures (ASME or AWS). If viewed as a method to control distortion then perhaps it would not need to be addressed as an essential variable whereas a method of post weld stress relief would most certainly have to be.
But my first question is - what is distortion control? is it a means to prevent stress in weldments thereby precluding the need for PWHT?
Secondly, if a qualified weld procedure on A36 mild steel called for no PWHT and a vibrational stress relief was applied anyway, does this violate the WPS?
Thankyou.