What is Utility grade aluminum

Status
Not open for further replies.

canwesteng

Structural
May 12, 2014
1,710
I've just come across a drawing calling for utility grade aluminum. Does anyone have any idea what this could be?
 
Replies continue below

Recommended for you

No idea. Utility grade is a low quality rating for wood.
 
Typically structural shapes are 6061-t6[highlight ][/highlight]
 
The "utility grade aluminum" that I'm acquainted with has at least 99.5% aluminum to maximize electrical conductivity, for use in wiring. It has a many decade history of use as conductors by "electric utilities". It is often alloy 1350. It can be made into sheets for other uses, but is softer than other alloys.

[idea]
[r2d2]
 
There is no utility grade. It means use the cheapest aluminum shapes available and the specifier does not care what the alloy is.
 
I believe SlideruleEra is right. We use aluminum for conductors and I don't have the specs in front of me but 1350 sounds right. I believe there are some aluminum castings used for the hardware that connects the conductors. Also wire splices are made from an aluminum alloy. Just this past weekend we had a splice fail that was installed in the line in 1955 that dropped a 138kV wire onto a distribution circuit that blacked out 15,000 homes for a couple of hours.

Prior to the 1960's a lot of copper was used in substations with copper fittings, but if you are a copper thief don't grab that old copper wire because it will definitely kill you.