Hi,

Can any one tell me what is toughtriding? Any litrature references?

Any help is appreciated.

Thanks,
Sk
 
The term is "Tuftriding". It is cyanide based nitriding process used a lot for automotive crankshafts.

Try Google using "Tuftriding" as the search term.
 