What is the partial pressure limit

Status
Not open for further replies.

ENGRANIA

Mechanical
Dec 17, 2008
34
What is the partial pressure limit of wet H2S for carbon steel at what temperature
 
Replies continue below

Recommended for you

What does the spec that you are working with say?
Each of the specs lists alloys and the limits for H2S, temp, pH, and other criteria.


= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
NACE 0175, as i want to use sa-179 hic material in gas cooler with 1000ppm at 275°f.
 
As much as you want if the carbon steel has the correct properties. This is from a cracking point of view. High H2S may cause other corrosion issues.

[URL unfurl="true"]https://res.cloudinary.com/engineering-com/raw/upload/v1678352593/tips/Interpretation_c12rtq.docx[/url]

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
As Mr. Jones pointed out, the NACE spec just addresses cracking.
You need to also consider all other forms of corrosion that might impact service.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
ENGRANIA said:
What is the partial pressure limit of wet H2S for carbon steel at what temperature
NACE MR0175 is a widely spread practice but actual limits depends on industry. What is your industry?
 
@ENGRANIA
This is an equipment type, not an industry. Check ISO 17945, ISO 21457, ISO 15156, NACE 8X194, NACE MR0103, NACE RP0296 for applicability. Note that standard applicable is affected by CO2 content and similar factors. Also para. 8 API 581 and DNVGL's report #14671 "Neutral and High pH SCC" might be useful.
 