Location
IN
thread378-183158
What is the NDE requirment as per ASME B 31.1 for closure welding joint (butt weld) ?
Please provide exact refrence if any ?
 
Thanks for your prompt reply,
I have gone through the Table 136.4, that is for the General NDE requirment, But i am insearch of Tie-in/ golden / closure Joint , whcih is not subjected to Hydrotest. Pl advice.
Regards
Aakash
 
Thanks phighfill,
For your prompt reply.
I have gone through the Table 136.4, This is for general requirment , BUt my question is Tie -in / Golden / Closure Joint, Whcih is not subjected to hydrotest.
Regrads
Aakash
 
There is not a special distinguish any special requirements for this type of inspection, all inspection is covered under the Table 136.4
 