Hello All
SA 350 LF2 flange (At the forging shop) is found to have discontinuity (16" 900 #) on the Flange OD. The Discontinuity cannot be left un attended. The forging has to be saved (Insted of rejection) by repair welding.
The location of the defect is 17mm from the OD and the depth of the defect is 13mm.
What should be considered as governing thickness "T" for the purpose of qualifying the weld procedure? Which clause of ASME SEC VIII and ASME Sec IX address such repair issues.
Governing thickness for the purpose of repair of Material is not found in ASME Sec VIII Div 1. UW 40 addresses weld repair and not the base material repair.
SA 350 LF2 flange (At the forging shop) is found to have discontinuity (16" 900 #) on the Flange OD. The Discontinuity cannot be left un attended. The forging has to be saved (Insted of rejection) by repair welding.
The location of the defect is 17mm from the OD and the depth of the defect is 13mm.
What should be considered as governing thickness "T" for the purpose of qualifying the weld procedure? Which clause of ASME SEC VIII and ASME Sec IX address such repair issues.
Governing thickness for the purpose of repair of Material is not found in ASME Sec VIII Div 1. UW 40 addresses weld repair and not the base material repair.