Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

What is the correct way to call out nylon 6/6 with 33% glass fill?

Status
Not open for further replies.

erabinowitz3

Mechanical
Sep 24, 2008
6
The way we mark an ABS part is: <ABS>

1) What is the name of the standard in which materials are called out this way?

2) to callout nyclon 6/6 with 33% glass fill, is it <PA66GF33> ?

Thanks
 
Replies continue below

Recommended for you

It is <PA66-GF33>.

The standards include:

ISO 1043-1—Plastics-Symbols—Part 1: Basic polymers and their special characteristics
ISO 1043-2—Plastics-Symbols—Part 2: Fillers and reinforcing materials
ISO 1629—Rubber and latices—Nomenclature
ISO 11469—Plastics—Generic identification and marking of plastic products
SAE J1344 MARKING OF PLASTIC PARTS

Regards,

Cory