Does any one know about the molecular sieve composition affecting the absorption ability?
The following data of 5A sieve from serching on the web:
0.80 CaO : 0.20 Na2O : 1 Al2O3: 2.0 ± 0.1 SiO2: x H2O
Does this mean I should get about 20 wt% of Ca ?
I'm interested in the absorption ability affecting by the Ca cation?
What is the tolarance of Cadium in 5A sieve?
The following data of 5A sieve from serching on the web:
0.80 CaO : 0.20 Na2O : 1 Al2O3: 2.0 ± 0.1 SiO2: x H2O
Does this mean I should get about 20 wt% of Ca ?
I'm interested in the absorption ability affecting by the Ca cation?
What is the tolarance of Cadium in 5A sieve?