Apr 24, 2006 #1 engtalal Mechanical Joined Oct 29, 2003 Messages 11 Location SA what is the a suitable STELLITE ELECTRODE can be used for SS304 material due the required material is not avaliable in our market STELLITE – 6. Can be used alternative STELLITE – 12 insted of STELLITE – 6? Regard
what is the a suitable STELLITE ELECTRODE can be used for SS304 material due the required material is not avaliable in our market STELLITE – 6. Can be used alternative STELLITE – 12 insted of STELLITE – 6? Regard
Apr 25, 2006 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Depending on service conditions (galling or abrasion), I would consider Stellite 21 or even Nitronic 60. What is your service application? Upvote 0 Downvote