what is the a suitable STELLITE ELECTRODE can be used for SS304 material due the required material is not avaliable in our market STELLITE – 6.
Can be used alternative STELLITE – 12 insted of STELLITE – 6?

Regard
 
Replies continue below

Recommended for you

Depending on service conditions (galling or abrasion), I would consider Stellite 21 or even Nitronic 60. What is your service application?
 