Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

What is the best method calculation for corrosion allowance in storage tank (water)?

Status
Not open for further replies.

Figueredo

Materials
Joined
Dec 11, 2013
Messages
26
Location
VE
What is the best method calculation for corrosion allowance in storage tank (water)?

thanks for the help.
 
Corrosion allowance is not something you calculate. It all depends on you process medium, your material of construction, your temperature, and industry experience with these conditions. Provide these and we'll be able to assist.
It's not a calculation but sort of a rule of thumb.
 
Start with looking at the difference between the minimum retirement thickness and the minimum thickness of the tank plate for construction so that you don't add steel on unnecessarily. Some standards give you a minimum corrosion allowance and you will have to make a call on whether that is sufficient based on expected corrosion rate and the corrosion control measures such as lining and cathodic protection. EEMUA 183 points out issues of low cycle fatigue in the annular section and recommends keeping it as thin as possible, suggesting a maximum corrosion allowance of 2mm for plate not exceeding 12.5 mm, and 1mm for thicker plate. Also, bear in mind that the usual corrosion morphology is pitting for which increased corrosion allowance doesn't offer a reliable barrier.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 