I'm trying to find out the EN designations of a few steel types from the old DIN norm but one of them I just can't find - and actually never heard of.
I know St 37 becomes S235, but what is St 37.0? Is it the same as St 37?
 
St 37.0 is essentially the same as St 37. The Werkstoff Nummer is 1.0254. This grade appeared in DIN 1626, DIN 1629, DIN EN 10216-1 (Draft version), and DIN EN 10217-1 (Draft version). It was also called P235T1. The composition is as follows:

C = 0.17 max
P = 0.040 max
S = 0.040 max
N = 0.009 max
 