Apr 3, 2006 #1 Cee555 Mechanical Joined Aug 30, 2005 Messages 49 Location CA What is NACE RPO472? I have a specification stating that all welds must meet requirements of NACE RP0472. Please help.
What is NACE RPO472? I have a specification stating that all welds must meet requirements of NACE RP0472. Please help.
Apr 3, 2006 1 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US It is RP ZERO 472 http://www.nace.org/nacestore/assets/freestandardsreports/RP047205.pdf Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
It is RP ZERO 472 http://www.nace.org/nacestore/assets/freestandardsreports/RP047205.pdf Regards, Cory Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
Apr 3, 2006 Thread starter #3 Cee555 Mechanical Joined Aug 30, 2005 Messages 49 Location CA Cory you just saved my job!!! Upvote 0 Downvote