What is male/female socket weld?

Status
Not open for further replies.

ryanhu

Petroleum
Feb 22, 2010
12
Hi everyone

What is male/female socket weld?

Is that the same with male/female Threaded?

So the male socketweld is buttweld,Is that right?
 
Replies continue below

Recommended for you

Socket welded connections are a type of welded connection where there is a male component that slides into a female component and then a fillet weld is made between the shoulder of the female component and shank of the male component.

Please refer to ASME B16.11 for typical dimensions and details.
 
120mg7p.png
 
A male socket welding end does not normally have any reduction in outside diameter. The outside diameter is constant and a fillet weld is used. The official dimensions for socket welded components would be specified in ASME B16.11.
 
Would like to back up rneill's contribution, and add that you're looking at a valve that has a "normal" SW end (female) with the other being male.

Heather Smith
My interests: Alloy valves, duplex valves, super duplex valves, 6Moly valves, inconel valves, incoloy valves, alloy 20 valves and titanium valves.
 