What is C.I.R.? A type of rubber?

Status
Not open for further replies.

Andy22

Mechanical
Joined
Jul 15, 2003
Messages
19
Location
CA
I have a drawing that specifies 1/8" thick C.I.R. for a flange gasket material. I suspect that it is actually natural rubber but what does C.I.R. stand for?
 
Hi andy22,

only a guess. If you think it it natural rubber actually then C I R could -could !!- mean cis isoprene rubber which is the synthetic twin of NR.

HTH Berti
 
Per ASTM D1418 (Vol 9.0) CIIR is chloro-isobutene-isoprene (chlorobutyl). Maybe someone left out the second "I"?
 