Finish spec for a 360 brass part is mentioned as BRIGHT DIP on the drawing. Is it like PLATING or CHROMATE DIP? OR it is something else?

Thanks.
 
Replies continue below

Recommended for you

From what I understand, it is just a chemical polishing process, but I don't know much beyond that.