I AM LOOKING FOR THE MAKE UP OF ASTM A487 Gr 4Q. PLEASE LET ME KNOW EXACTLY WHAT I AM DEALING WITH. THANK YOU.
 
Replies continue below

Recommended for you

cast steel
11-13 Cr % and some nickel ....etc
 