Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

What is a "B" mark on Steel? 4

Status
Not open for further replies.

mann

Structural
Feb 17, 2000
16
I am looking at the plans for a steel frame and masonry building from 1964. Several of the beams use a notation as follows: 10 B 11.5. Is that a Wide flange section?
 
Replies continue below

Recommended for you

10B11.5 is a light weight rolled section similar in appearance to a WF section. They appear in the AISC Steel Handbook of Sixth Edition and earlier.

The properties are as follows:

Depth 9.87"
Flange Width 3.950"
Flange Ave Thk 0.204"
Web Thk 0.180"

Area 3.39
d/Af 12.3
Ixx 51.9
Sxx 10.5
rx 3.92
Iyy 2.01
Syy 1.02
ry 0.77
 
From the reference: Iron and Steel Beams 1873 to 1952 published by AISC, there were many designations given to beams before standard rollings were adopted. In other words, each steel mill would roll a slightly different shape. Some of the designations follow.

B - Bethlehem Steel Company
C - The Carnegie Steel Company, Ltd 1893 - 1896
C - Carnegie Steel Company 1900-1934
CA - Cambria Steel Company
CAM - Cambria Steel Company
CIL - Carnegie-Illinois Steel Corporation
CP - Carnegie Phipps & CO. Limited
IL - Illinois Steel Company
IN - Inland Steel Company
.
.
.
US - United States Steel Company

The above reference is invaluable for working with older structures as it not only contains properties but also stresses of those mill products.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor