I would like to know what a fan gate is and will it work on a plastic part. Is there an advantage if is will work on plastic molds.


Please respond.

Wayne Wickerham
 
Replies continue below

Recommended for you

A fan gate is a gate that "fans out" in one direction while narrowing to quite small in the other direction. both directions transverse to the flow. This is used ro avoid "jetting" whrn the part is shot and to spread the material out as it flows into the cavity when a flow like that is judged neccessary.
 
Fan gates are also useful in aplications that have a high flow length to wall thickness ratio ..... and long flat parts that could be prone to distortion. They can be considered a step between a tab gate and a film gate. But as Insideman says will also help solve jetting problems.

Be careful what you use them on as with some materials they can be a wast of time.