Feb 6, 2002 #1 faihin Mechanical Joined Oct 9, 2001 Messages 1 Location TH Please compare dracomet and hot dip.
Feb 6, 2002 #2 nashjp Mechanical Joined Sep 24, 2001 Messages 18 Location US I hope it is a misspelling of Dacromet. Dacromet is a brand name for coatings used for corrosion protection. Upvote 0 Downvote
I hope it is a misspelling of Dacromet. Dacromet is a brand name for coatings used for corrosion protection.
Feb 6, 2002 #3 Kenneth Aerospace Joined Jun 12, 2001 Messages 334 Location US See thread725-10280. Upvote 0 Downvote