What are the differences between a 304L and a 304PS stainless steel ? What does PS mean ? Are there difference on corrosion resistance ?
Thank you very much in adavance for your answers.
Mdev
 
Replies continue below

Recommended for you

marief
The only reference I have seen for PS is plasma spray application. In what context was 304 PS used?
 
I think it is either precision strip or pipe, sanitary. This isn't one of the standardized designations, as far as I know.

Regards,

Cory