Aug 30, 2004 #1 mahadhatu Materials Joined Nov 4, 2003 Messages 65 Location US Dear Gurus, I have been trying to find out what is 304D type stainless steel. We have a customer who has specifically mentioned that they do not want a 304D type SS for their part. Can some one throw some light on this? Thank you, Mahadhatu.
Dear Gurus, I have been trying to find out what is 304D type stainless steel. We have a customer who has specifically mentioned that they do not want a 304D type SS for their part. Can some one throw some light on this? Thank you, Mahadhatu.
Aug 30, 2004 #2 codeeng Petroleum Joined Feb 9, 2004 Messages 365 Location CA Probably means dual certified i.e. meeting both type 304 and 304L SS Upvote 0 Downvote
Aug 31, 2004 Thread starter #3 mahadhatu Materials Joined Nov 4, 2003 Messages 65 Location US Thank you Codeeng, That was my guess too. I havent found it written any where yet. so I am still looking. Thank you for your input. Upvote 0 Downvote
Thank you Codeeng, That was my guess too. I havent found it written any where yet. so I am still looking. Thank you for your input.
Aug 31, 2004 #4 codeeng Petroleum Joined Feb 9, 2004 Messages 365 Location CA Try this supplier. They list 304D coming from Europe. http://www.paramounttrading.com/aboutus.html Upvote 0 Downvote