screenzzzz
Industrial
- Dec 16, 2006
- 7
I'm looking for some feedback on what is the fastest way to cure a flat piece of pvc gel. the options I see are.
a. blow heat directly on top of it at max temp it can take
b. teflon coated hot plate on top of it at curing temp.
.040" thick 4" diameter circle of pvc gel. on a teflon coated aluminum plate
the purpose is to cure it
curing temp 325F.
I am trying to force cure as fast as possible w/o, scorching the surface. is the scorching point based only on a higher temperature than the curing temp?
are there other ways of curing than described?
a. blow heat directly on top of it at max temp it can take
b. teflon coated hot plate on top of it at curing temp.
.040" thick 4" diameter circle of pvc gel. on a teflon coated aluminum plate
the purpose is to cure it
curing temp 325F.
I am trying to force cure as fast as possible w/o, scorching the surface. is the scorching point based only on a higher temperature than the curing temp?
are there other ways of curing than described?