We are in the process of analyzing an existing filigree slab. On the exisiting design drawings there is a note point to the top layer with the designation S.H. CONCRETE. Does this mean anything to anyone? The drawings are from the late '70s.
 
Surface Hardened.
 
Is surface hardening the same thing as when they put hardening powder on the surface of a slab....like in a machine shop?
 
Tim76...yes. I can be in the form of a "dry shake" done at the time of finishing or can be done as a separate hard topping over the base slab.
 
You have read the specifications pretty carefully because there are a wide variety of surface applied hardeners ranging from liquid to dry shake-ons. The costs vary widely too. Dry shake-ons like Master Plate can get very expensive for both material and labor, but have their specialty uses.
 