iam42
Industrial
- Feb 15, 2007
- 175
I have a joint that is a single v between two pieces of carbon steel pipe. Inside the pipe is a stainless steel nozzzle which is incorporated into the weld like a backing material.
My question is..... should this be classified as a P1 to P1 weld or a P1 to P8 weld, secondly, what consumable classification would you use to weld it. 309 or 70XX?
I have attached a sketch which may help in understanding my poor description above.
Thanks
My question is..... should this be classified as a P1 to P1 weld or a P1 to P8 weld, secondly, what consumable classification would you use to weld it. 309 or 70XX?
I have attached a sketch which may help in understanding my poor description above.
Thanks