Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

what are the hyperelastic materials used in aircraft

Status
Not open for further replies.

arivu006

New member
Nov 5, 2011
1
application of hyper elastic materials used in aircraft?
 
Replies continue below

Recommended for you

Please tell us what you mean by hyper elastic..


Mike Halloran
Pembroke Pines, FL, USA
 
You know - the ones that get really really excited about stretching.


I've never seen any on an aircraft; eyeglasses maybe.

I'm starting to think EngTips needs some sort of moderation for first time posters. Too many poorly formed questions which sound suspiciously like undergrad homework questions.
 
Well, rubber for tires, seals, some hoses, as a f'rinstance.
 
i think British Aerospace uses super-plastically-formed Ti to make the access panels on Airbus wings. does that count ?
 
Wouldn't super plastic be different from super elastic? Super plastics have a number of applications.
 
Rubber is also used in constrained-layer damping...when needed.
 