What are the best piping materials can be used for stem line 115 psi pressure and 340 degrees Fahrenheit??
 
Replies continue below

Recommended for you

The best and most acceptable material shall be carbon steel, and the pipe to specification ASTM A106 Grade A or B. I presuem that schedule 40 will be safe to be used.

Narendra K. Roy
Gramya Research Analysis Institute,
PO box 4016, Vadodara 390015, India
Website: ;
 