I want to increase the hardness of polyurethane for making parts via injection molding. The material I have is one-component polyester urethane based on an aromatic diisocyanate in granule form. It's hardness is 80 Shore A.
What additive can i mix with the granules to get a harder product after injection molding?
Is there any additive/material that I can use with my granules to harden them by twin screw extrusion/compounding?
 
Replies continue below

Recommended for you

Carbon black?

Seriously, why not source a harder durometer material?
 
Anything with higher hardness than the PU which means just about anything.

Calcium carbonate, talc, mica, wollastonite, silica, barium sulfate etc. etc.

Contact a mineral filler supplier.

Chris

Chris DeArmitt - PhD FRSC CChem
Plastic & Additives Webinars
Instant Downloads & Inexpensive
 
You could compound it with a 60 Shore D material (about the stiffest grade). You would get some intermediate hardness depending on mix ratio.

H




Why be happy when you can be normal?
 
Urethane PBT copolymers are harder and are available as Arnitel and Hytrel. There are others, but you can look them up as easily as I can.

Regards
Pat